Steam Oxidation of Modified Silicon/Ytterbium Disilicate Environmental Barrier Coatings on SiC/SiC Ceramic Matrix Composites at 1250-1350 °C (OCT, 10.1007/s11666-025-02101-5, 2025) Correction (Web of Science) Early Access (Web of Science)